Oxidation State Of Manganese Ions In Silicate Gels And Gel-Derived Glasses

In the present work 0.5Mn0-99.5Si02,0.5Mn0-5Al203 and 0.5Mn0-5Ca0-94.5Si02 gels and gel derived glasses prepared by using tetraethylorthosilicate (TEOS) and manganese, calcium and aluminium nitrates as starting materials were studied.

Author
M G Ferreira Da Silva & J Rocha
Origin
Universidade De Aveiro, Portugal
Journal Title
Phys Chem Glasses 39 1 1998 41-44