An Overview Of Alumina-Silica Refractories And Their Advantages

In this article the authors outline the advantages and disadvantages of alumina-silica refractories and unveil the latest research aimed at increasing the service life and improving the alkali resistance of the high alumina grades utilised in the regenerator stack.