Overall Coeficients For Flat Glass Determined Under Naturla Weather Conditions.

Data are given for tests made under natural weather conditions on a single sheet of glass and on two sheets spaced 0.25 in apart. Test were made with the glass exposed to wind velocities of 3 to 9 miles per hour and with the glass sheltered from the wind. Surface conductance's have been analysed and show the separate influence of convection and radiation, the latter including nocturnal radiation effects. Comparisons are made with hot box test data.

Author
G.V. Parmelee And W.W. Aubble
Origin
Unknown
Journal Title
Heating Anf Piiping And Air Conditioning, 20 [12] 111-18 (1948).
Sector
Primary Papers
Class
PP 323

Request article (free for British Glass members)

Overall Coeficients For Flat Glass Determined Under Naturla Weather Conditions.
Heating Anf Piiping And Air Conditioning, 20 [12] 111-18 (1948).
PP 323
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.