Our Heritage Of Stained Glass And Its Care In The 2Oth Century

A brief account is given of the origins and work of the York Glaziers' Trust. The restoration of York Minster's Rose Window following damage suffered in the fire of 9 July 1984 is described.

Author
P Gibson
Origin
Unknown
Journal Title
Glass Technol 1988 29 6 218-225
Sector
Flat glass
Class
F 102