Origin Of Absorption Bands Observed In The Spectra Of Silver Ion-Exchanged Soda-Lime-Silica Glass

The spectral absorption of Ag-containing soda-lime-silica glasses, prepared by ion exchange under different conditions and subjected to different heat treatments, was measured in the UV and the visible. Tentative Gaussian resolution analysis was performed to accurately define the component bands of the experimentally observed absorption spectra.

Author
A A Ahmed & E W Abd Allah
Origin
Nat Res Centre, Cairo, & Tanta University, Tanta, Egypt
Journal Title
J Am Ceram Soc 78 10 1995 2777-2784
Sector
Special Glass
Class
S 935

Request article (free for British Glass members)

Origin Of Absorption Bands Observed In The Spectra Of Silver Ion-Exchanged Soda-Lime-Silica Glass
J Am Ceram Soc 78 10 1995 2777-2784
S 935
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.