Oriented Crystallisation Of Lithium Niobate Containing Glass Ceramic In An Electric Field And Determination Of The Crystallographic Orientation By Infrared Spectroscopy

A glass melt with the composition (mol%) 45Li20, 20Nb205 and 35Si02 was soaked at 1000 deg C. This did not lead to any crystallisation. A current of 50mA applied between the platinum crucible (anode) and a platinum wire inserted into the melt (cathode) resulted in a crystallisation of LiNb03, Li2Si203, Li2Si205 and Li2Si03 at the cathode. The resulting glass ceramic showed textured structures which indicate dentritic growth.

Author
K Gerth Et Al
Origin
Otto-Schott Inst, Germany
Journal Title
Phys Chem Glasses 40 3 1999 135-139
Sector
Glass Ceramics
Class
GC 360

Request article (free for British Glass members)

Oriented Crystallisation Of Lithium Niobate Containing Glass Ceramic In An Electric Field And Determination Of The Crystallographic Orientation By Infrared Spectroscopy
Phys Chem Glasses 40 3 1999 135-139
GC 360
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.