Organic Inks From Ppg Industries

PPG Industries has developed a new line of EcoBrite organic inks for glass decorating offering a line of easy-to-use, thermally-cured, heavy metal-free inks that can replace traditional ceramic inks in decorating glass bottles & related items. EcoBrite organic inks can print multicolour designs & provide several important benefits. They are formulated to be free of toxic heavy metals & have been designed to be screenprinted using existing commercial bottle decorating equipment & cured in existing lehrs. The inks cure at low lehr temps (~180 deg C), resulting in significant energy savings. In contrast to traditional ceramic inks, they do not weaken the structural integrity of the glass container. As a result, bursting pressure of bottles decorated with EcoBrite inks is higher than that of similar bottles decorated with ceramic inks.

Author
Un-named
Origin
Unknown
Journal Title
Glass International Jan/Feb 2005 28
Sector
Container glass
Class
C 2561

Request article (free for British Glass members)

Organic Inks From Ppg Industries
Glass International Jan/Feb 2005 28
C 2561
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.