Optimum Composition Of Blast Furnace Slag As Deduced From Liquidus Data For The Quarternary System Cao-Mgo-A203-Si02

On the basis of liquidus measurements in the system CaO-MgO-Al203-Si02 and previously published data, diagrams have been constructed at 5% Al203 intervals from 5-35% Al023. Liquidus temperatures and primary phase fields are shown. The optimum composition of a blast furnace slag for a given alumina content is indicated. At the optimum point, ordinary slags will be entirely liquid and will have maximum desulphurization potential and minimum viscosity.

Author
E F Osborn Et Al
Origin
Unknown
Journal Title
J Metals January 1954 33-45
Sector
Primary Papers
Class
PP 82

Request article (free for British Glass members)

Optimum Composition Of Blast Furnace Slag As Deduced From Liquidus Data For The Quarternary System Cao-Mgo-A203-Si02
J Metals January 1954 33-45
PP 82
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.