Optimizing The Christiansen-Shelyubskii Method And Its Comparison With Industrial Control Methods For Homogeneity Determination Of Glasses

The Christiansen-Shelyubskii method used in this work was optimized experimentally. Different tests were performed with two grain fractions of standardized crushed sheet glass. Maximum transmissions, half-widths and their standard deviations were optimized and it was further shown that sampling, an appropriate cleaning of the granulated glass, and the quality of the optical cells used are of great importance.

Author
R P Heidrich & G H Frischat
Origin
Inst Nichtmetallsche & Tech Univ Clausthal, Germany
Journal Title
Glastech Ber Glass Sci Technol 72 6 1999 197-203
Sector
Special Glass
Class
S 1677

Request article (free for British Glass members)

Optimizing The Christiansen-Shelyubskii Method And Its Comparison With Industrial Control Methods For Homogeneity Determination Of Glasses
Glastech Ber Glass Sci Technol 72 6 1999 197-203
S 1677
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.