Optimization Of Oxy-Fuel Combustion With Optical Sensors

In this paper a novel method for monitoring and controlling oxy-fuel burners by strategic placement of optical sensors is presented. The sensors are integrated into an industrial oxy-fuel burner capable of withstanding harsh environments.