Optimization Of Compositions And Properties Of Silver-Free Photochromic Glasses

It is shown that optimization of the compositions and properties of photochromic glasses by standard parameters does not always give an optimum result because it is often necessary to use nonstandard reference parameters in addition to the standard ones in order to take into account all of the standard properties.

Author
Yu I Mashir
Origin
Unknown
Journal Title
Glass & Ceram 53 5-6 1996 196-199