Optimization Of Composite Leaf Spring Design Using Response Surface Methodology

The advancement in fibre composite technology puts back many dense materials by high strength to density ratio. Many attempts have been made with glass/carbon fibre for suspension systems; still, not much has been done in the direction of optimisation of the design of the leaf spring. This paper reports on the work in which a new glass/carbon fibre composite material was made and tested under Tsai-Wu failure stress criteria.

Author
S Rajesh Et Al
Origin
Tagore Eng College, Chennai, India
Journal Title
Romanian J Materials 47 1 2017 98-105
Sector
Glass Fibre
Class
GF 739

Request article (free for British Glass members)

Optimization Of Composite Leaf Spring Design Using Response Surface Methodology
Romanian J Materials 47 1 2017 98-105
GF 739
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.