Optimisation Of Melting Parameters And Minimizing Oh Content In Sio2-B2O3-Na2O-Bao Glass System In Microwave Heating

This study investigates the optimisation of melting process for the glass comprising SiO2-B2O3-Na2O-BaO under microwave heating (MW). Batches were melted at different temperatures in the range of 900-125 deg C to optimise melting conditions. XRF suggests amorphous nature of samples melted above 1150 deg C. Optimisation of melting time was carried out by varying soaking time (8-60m) at 1250 deg C. UV-Vis-NIR spectra level reveal ~90 transmission over 300-2000 nm wavelength range for glass melted at 1250 deg C. Optical microscopic images suggest that the bubble-free glass can be produced at 1250 deg C for 1 hour melting in MW heating. MW heating also helps in reducing OH content in glass. However, OH concentration is found to increase with melting time.

Author
A K Mandal, R Sen
Origin
Csir, Kolkata, India
Journal Title
Int J Appl Glass Sci January 2019 83-91
Sector
Special Glass
Class
S 4500

Request article (free for British Glass members)

Optimisation Of Melting Parameters And Minimizing Oh Content In Sio2-B2O3-Na2O-Bao Glass System In Microwave Heating
Int J Appl Glass Sci January 2019 83-91
S 4500
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.