Optimisaiton Of The Use Of Raw Materials To Obtain The Best Efficiency Results: Evaluation Of The Chemical And Physical Aspects

Studies are done to compare an initial situation, based on the use of silica sands associated with various alumina carriers, and a final situation which considers the use of the Gruppo Minerali's feldspathic sands, alone or combined with traditional silica sands. Another case considers the addition of Vitrite blast furnace slags in the production of flint as well as coloured glasses.

Author
C Ferrero
Origin
Gruppo Minerali Spa, Italy
Journal Title
Int Glass Journal No 107 Jul-Aug 2000 31-36
Sector
General
Class
G 2270

Request article (free for British Glass members)

Optimisaiton Of The Use Of Raw Materials To Obtain The Best Efficiency Results: Evaluation Of The Chemical And Physical Aspects
Int Glass Journal No 107 Jul-Aug 2000 31-36
G 2270
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 17 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.