Optimal Control Strategy For Predictive Compensation Of Gas Quality Fluctuations In Glass Melting Furnaces

The German glass industry is facing increasing problems born from fluctuating composition of natural gas. For cost optimization, gas suppliers are frequently switching between different sources of natural gas, taking bio gas from local sources too. In the near future we may expect hydrogen from windmills as well. This paper presents a strategy for balancing different sources of gases used and their quality for glass melting.

Author
P Hemmann
Origin
Society of Glass Technology Combustion Control Gmbh, Germany
Journal Title
77 Conference On Glass Problems 2017 55-63
Sector
General
Class
G 4611

Request article (free for British Glass members)

Optimal Control Strategy For Predictive Compensation Of Gas Quality Fluctuations In Glass Melting Furnaces
77 Conference On Glass Problems 2017 55-63
G 4611
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.