Optical Spectroscopy Of A Soda-Lime Glass Exchanged With Silver

A commercial flat soda lime glass subjected to an ion exchange process with Ag+ at different temperatures for different lengths of time is investigated by means of transmission electron microscopy (TEM), optical absorption (OA) and photoluminescence (PL) techniques.