Optical Spectroscopy Of Ce3+, Tb3+ And Eu3+ In New Scintillating Glasses

Optical absorption, luminescence and excitation spectra of new silicate scintillating glasses doped with Eu3+, Ce3+ and Tb3+ have been measured at room temperature.