Optical Properties Of Window Glass In The 40 To 630 Deg C Temperature Range At Wavelengths From 2.0 To 4.3Um

The optical properties of float window glass in the 2300-5000 cm-1 region at temperatures from 40-630 deg C are investigated. The absorption spectra are measured with a high-temperature accessory. The spectra of the optical constants, individual components of the absorption spectra, and also the band frequencies and intensities are calculated with the dispersion analysis method. The effect of temperature on the spectra is shown to be due to changes in the intensities of certain water-related bands. The most important intensity changes are discussed in terms of the reversible shift of an equilibrium between different structural sites for the hydroxyl group.

Author
A M Efimov & P A Van Nijnatten
Origin
Vavilov State Optical Inst (Russia) & Tno, Netherlands
Journal Title
Glass Sci Technol 76 5 2003 213-219
Sector
Flat glass
Class
F 1499

Request article (free for British Glass members)

Optical Properties Of Window Glass In The 40 To 630 Deg C Temperature Range At Wavelengths From 2.0 To 4.3Um
Glass Sci Technol 76 5 2003 213-219
F 1499
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.