Optical Properties Of Transparent Glass-Ceramics Containing Er3+ -Doped Sodium Lutetium Fluoride Nanocrystals

Transparent glass-ceramics containing Er3+-doped sodium lutetium fluoride nanocrystals for photonic applications have been synthesized. Glass transition temperature, softening temperature, and crystallisation temperature were estimated by dilatometry and differential thermal analysis. Proper heat treatments were selected to crystallise lutetium fluoride nanocrystals. X-ray diffraction analysis was carried out to identify the crystalline phase and the crystal size. HRTEM indicates that the base glass is phase separated in droplets enriched in Lu, Na, F and also Er ions. The thermal treatment induces the crystallisation inside the droplets. The optical characterisation, which includes absorption and steady-state and time-resolved emission spectroscopy under one- and two-photon excitation, shows the differences between the phase-separated base glass and its corresponding glass-ceramic. The reduction of the Judd-Ofelt parameter, together with the increase of the fluorescence lifetimes as compared to the glass sample confirms the presence of Er3+ ions in a crystalline environment in the glass-ceramic samples. Moreover, an enhancement of the green and red up-converted emissions (as well as the weak blue emission) is observed int he glass-ceramic, indicating the Er3+ incorporation into the nanocrystals.

Author
M J Pascual Et Al
Origin
Inst Ceramics Y Vidrio, Madrid, Spain
Journal Title
Int J Appl Glass Sci 7 1 2016 27-40
Sector
Glass Ceramics
Class
GC 880

Request article (free for British Glass members)

Optical Properties Of Transparent Glass-Ceramics Containing Er3+ -Doped Sodium Lutetium Fluoride Nanocrystals
Int J Appl Glass Sci 7 1 2016 27-40
GC 880
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.