Optical Properties Of Sodium Fluoroborate Glasses Containing Pr3+ Ions For Red Luminescence

The luminescence properties of sodium fluoroborate (SFB) glasses containing different concentrations of Pr3+ ions were characterized through optical absorption, emission and decay measurements. From the measured intensities of various absorption bands of 1.0 mol% Pr3+ ions, the Judd-Ofelt intensity parameters were determined by including and excluding the 2H4>3P2 hypersensitive transition.

Author
D Umamaheswari Et Al
Origin
Sri Venkateswarea Univeristy, Tirupati, India
Journal Title
Phys Chem Glasses 53 6 Dec 2012 271-275
Sector
Special Glass
Class
S 3963

Request article (free for British Glass members)

Optical Properties Of Sodium Fluoroborate Glasses Containing Pr3+ Ions For Red Luminescence
Phys Chem Glasses 53 6 Dec 2012 271-275
S 3963
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.