Optical Properties Of Pr3+ Ions In Lithium Borate Glasses

The absorption spectra of Pr3+ are studied inthe following lithium borate glasses: MCO3+Li2CO3+H3B03, where M=Mg, Ca, Sr and Ba. The observed band positions are analysed in terms of a parameterised Hamiltonian model that consists of 14 interaction parameters of atomic nature.

Author
A R Devi & C K Jayasankar
Origin
Sri Krishnadevaraya University Post-Grad Centre , India
Journal Title
Phys Chem Glasses 37 1 1996 36-40