Optical Properties Of Glazing Materials At Normal Incidence

Measurements of spectral transmittance T and reflectance R at normal incidence continue to be the most common and accurate source of energy performance data for glazing materials. Prediction of these radiometric properties from more fundamental materials data is often confounded by the complexity and uncertainty of coating structures. Angle-dependent radiometric properties of coated glazing will probably be predicted from normal-incidence data rather than being measured at many angles. The general error level demonstrated in round-robin tests is in the order 1-2%; it is often necessary to achieve better levels of performance. Based on results obtained following the round-robin tests, an accuracy of better than 0.5% can be generally achieved. A new type of absolute standard reference is described and tested with promising results.

Author
M Rubin & R Powles
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 31 1 2001 13-16
Sector
Flat glass
Class
F 1223

Request article (free for British Glass members)

Optical Properties Of Glazing Materials At Normal Incidence
Riv Staz Sper Vetro 31 1 2001 13-16
F 1223
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.