Optical Properties Of Glasses In The System Ca0-A1203-B203

The optical properties of Ca0-Al203-B203 glasses are reported in this paper. The variation of refractive index, dispersion, ultra-violet absorption and density with composition is in agreement with previously published results on dielectric properties. Inflections in physical property curves are discussed in terms of formation of non-bridging oxygens. Infrared spectroscopy suggests the presence of boroxol groups up to 40 mol% Ca0. The tetraborate groups gradually diminish on increasing Ca0 concentration higher than 25 mol%.

Author
R Kudesia Et Al
Origin
Alfred University, New York, Usa
Journal Title
Schott Research 1993-1995 119-128
Sector
Special Glass
Class
S 1163b

Request article (free for British Glass members)

Optical Properties Of Glasses In The System Ca0-A1203-B203
Schott Research 1993-1995 119-128
S 1163b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.