Optical Properties Of Dysprosium-Doped Low-Phonon-Energy Glasses For A Potential 1.3Um Optical Amplifier

Dypsrosium-doped glasses were prepared in the system of gallium-based sulphide, tellurite, zirconium-based and indium-based fluorides and their optical properties were studied.

Author
S Tanabe Et Al
Origin
Kyoto University, Japan
Journal Title
J Am Ceram Soc 78 11 1995 2917-2922