Optical Bonding Of Tellurite Glass Film On Silicate Glass

Tellurite glass thin film was successfully bonded on a silicate glass substrate by the direct-bonding (DB) method. Glass film (1-3um) was fabricated by the glassblowing technique and the DB process was performed at room temperature at relative humidity (RH) of 62% or 15%. The surface adhesive strengths of the glass films bonded at 15% and 62% RH were measured as 250 and 96 mJ/m2, respectively, by the Obreimoff-Metsik method. The hydroxl (-OH) functional groups on the interface between the film and silicate glass were analysed by Fourrier thin film and silicate glass were hydrogen bonds at 62% RH and bonds between Te on the tellurite glass and O on the silicate glass were concerned at 15% RH. These forces, contributed by Si-OH, were important for bond formation at 62%.

Author
R J Jeng Et Al
Origin
Tokyo Inst Technology, Japan
Journal Title
Int J Applied Glass Science 10 2019 248-258
Sector
Special Glass
Class
S 4523

Request article (free for British Glass members)

Optical Bonding Of Tellurite Glass Film On Silicate Glass
Int J Applied Glass Science 10 2019 248-258
S 4523
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.