Optical Basicity Analysis Of Glasses Containing Trivalent Scandium, Yttrium, Gallium And Indium

Refractivity data of the following ternary glasses were used to obtain the molar electronic polarisability of each glass: Sc2O3-Na2O-SiO2, Y2O3-Na2O-SiO2, In2O3-NaO-SiO2, Ga2O3-M2O-SiO2 (where M is Li or Na) and Ga2O3-MO-SiO2 (where M is Ca, Sr or Ba).