Optical And X-Ray Absorption Spectroscopies Of Iron In Minerals And Glasses: Experiment And Theory

As iron is the most abundant transition element, understanding the crystal chemistry of Fe2+ and Fe3+ in minerals and glasses remains an important issue. This paper presents an extensive set of data on the spectroscopic properties of 12Fe2+ and Fe3+ minerals, using two kinds of techniques: synchrotron-based high-resolution X-ray spectroscopy, and optical absorption spectroscopy.

Author
G Lelong Et Al ([email protected])
Origin
Institute Of Mineralogy, Impmc, France
Journal Title
13Th Symp Eu Soc Of Glass Science 2016 172
Sector
General
Class
G 4564a

Request article (free for British Glass members)

Optical And X-Ray Absorption Spectroscopies Of Iron In Minerals And Glasses: Experiment And Theory
13Th Symp Eu Soc Of Glass Science 2016 172
G 4564a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.