Online Fire Polishing: Pre-And Post Mix Approaches

With today's increasing demands on glass surface quality and consistency, it has become necessary to develop technology capable of achieving a hand crafted finish at a machine finished cost. This article explains how it is possible to improve surface quality and consistency without sacrificing productivity with its online pre-and post mixing burners.

Author
G Rush & M Goerisch
Origin
Linde Group
Journal Title
Glass International May 2009 45-46
Sector
Container glass
Class
C 3953

Request article (free for British Glass members)