A One-Step Forming Process For The Glass Container Industry

The glass industry is facing many problems of which probably the most decisive aspects are the reduction of energy and emissions. A strategic answer is a one-step forming process for high mechanically resistant, thin glass containers. Beside an increase in the mechanical properties, the stabilisation of the container production process is a major task together with some new developments such as a combined press and blow process. The advantages arising from this overall process will benefit other sectors of the glass industry.

Author
H Hessenkemper
Origin
Tu Bergakademie Freiberg, Germany
Journal Title
Gmpa 6/05 70-73
Sector
Container glass
Class
C 2849b

Request article (free for British Glass members)

A One-Step Forming Process For The Glass Container Industry
Gmpa 6/05 70-73
C 2849b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.