Od Bands In The Ir Spectra Of A Deuterated Soda-Lime-Silica Glass

IR spectra of a deuterated glass of the composition (in mol%) 16Na20.10CaO.74Si02 complete earlier spectroscopic studies on water-poor soda-lime-silica glasses. The approved IR spectroscopic method of the deuterium exchange allows a reliable assignment of the hydroxyl bands also in the case of glasses. By spectra comparison the assignment of the IR bands at 2500 and 2800cm -1 to hydroxyl groups with different hydrogen bonding is verified.

Author
C Peuker Et Al
Origin
Bundesanstalt Fur Materialforschung, Berlin
Journal Title
Glastech Ber Glass Sci Technol 74 7 2001 210-214
Sector
Special Glass
Class
S 2243

Request article (free for British Glass members)

Od Bands In The Ir Spectra Of A Deuterated Soda-Lime-Silica Glass
Glastech Ber Glass Sci Technol 74 7 2001 210-214
S 2243
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.