Occupational Exposure To Optical Radiation And The Occular Health Status Of Glassblowers'

The occupational radiation exposure levels and the ocular health status of a sample of glass-blowers in southern Ontario were evaluated. The form of ocular protection was also assessed. Measurements of radiant emissions from different molten glass materials were carried out. A total of six glassblowing installations, 15 glassblowers and 42 non-glassblowers participated in the study. The spectral transmittances of samples of the protective lenses were obtained. Tonometry, biomicroscopy, ophthalmoscopy, pachometry, Schirmer tear test, endothelial photography were completed on all the volunteering subjects. The glassblowers ocular findings were compared to those of non-glassblowers. No indication of cataract was observed among this group of glassblowers. Although, a preponderance of grade 2 polymegethism among the glassblowers (47% compared to 11% in non-glassblowers) was found, there was no significant difference in their ocular health. Variation in the corneal irradiance from the occupational exposure was obtained, and in addition, the use of protective lenses was found to be inappropriate. In order to prevent against any long-term chronic pathological effect, the use of appropriate ocular protection is advised.

Author
O M Oriowot Et Al
Origin
University Of Waterloo, Ontario, Canada
Journal Title
Ophthal Physiol Opt 17 6 1997 483-491
Sector
General
Class
G 3960

Request article (free for British Glass members)

Occupational Exposure To Optical Radiation And The Occular Health Status Of Glassblowers'
Ophthal Physiol Opt 17 6 1997 483-491
G 3960
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.