Observation Of A Raman-Induced Interpulse Phase Migration In The Propagation Of An Ultrahigh-Bit-Rate Coherent Soliton Train.

Coherent soliton packets generated in a passively mode-locked fiber laser are transmitted through 23km of dispersion-decreasing fiber. We observe a shift of the phase difference between solitons that is due to intrapulse Raman scattering. We attribute the stability in propagation of these trains to a trade-off between minimizing soliton-soliton interactions by reduction of the pulse width and minimizing this Raman-induced phase migration, which can force the solitons into a deleterious attractive phase relationship. We are thus able to demonstrate the propagation of 177-Gbit/s soliton packets over a distance of 123 soliton periods.

Author
E L Buckland, R W Boyd & A F Evans
Origin
University Of Rochester & Corning New York
Journal Title
Corning Research 1997 101-103
Sector
Special Glass
Class
S 1449

Request article (free for British Glass members)

Observation Of A Raman-Induced Interpulse Phase Migration In The Propagation Of An Ultrahigh-Bit-Rate Coherent Soliton Train.
Corning Research 1997 101-103
S 1449
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.