Objective Measurement Of Residual Stresses

Mechanical stresses can impair the fracture strength and processing ability of glass products. Testing for residual stresses is therefore an important constituent of quality control In this article, the author Henning Katte from German-based Ilis, explains a new way of measuring glass stresses in real time.