O-I Forms University R&D Partnership

O-I has signed a three year agreement with the University of Toledo College of Engineering, Chemical & Environmental Engineering Department, to support research at O-Is new R&D Innovation Centre. The new centre is set to be completed by autumn 2013. It will produce sample glass containers using new manufacturing technologies and product designs being tested by the company. The agreement covers salary and fees for graduate research assistance to partner with O-I scientists and engineers. It also covers the purchase of equipment specific to characterise glass, and fees to use UT's equipment, including x-ray diffraction and scanning electron microscopy instruments.

Author
Un-named
Origin
Unknown
Journal Title
Glass International March 2013 3
Sector
Container glass
Class
C 4851

Request article (free for British Glass members)

O-I Forms University R&D Partnership
Glass International March 2013 3
C 4851
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.