Numerical Simulation Of Bubble Behaviour In Glass Melting Tanks. Part 1. Under Ideal Conditions

The presence of bubbles in the final glass is one of the main defect problems faced by the glass industry. Because of bubbles a sizeable proportion of glass products may need to be recycled before leaving the plants causing considerable waste of energy, time and financial resources. Therefore, understanding bubble behaviour in glass melts is a very important first step in attempting their reduction in the final glass. The overall objective of this study was to contribute to these efforts by analysing the problem in four parts.

Author
B Balkanli & A Ungan
Origin
Purdue University School Of Eng & Technology, Indianapolis, Usa
Journal Title
Glass Technology 37 1 1996 29-34
Sector
General
Class
G 1405

Request article (free for British Glass members)

Numerical Simulation Of Bubble Behaviour In Glass Melting Tanks. Part 1. Under Ideal Conditions
Glass Technology 37 1 1996 29-34
G 1405
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.