Numerical Approach To Fracture Of Glass Under Biaxial Stress

The fracture behaviour of brittle materials under biaxial plane stress has been investigated by means of numerical simulation method with software MFPA (Material Failure Process Analysis). The aims of this study are to clarify the fracture dependence of brittle material on biaxial plane stress state. The observation of crack initiation and fracture behaviour reveals that the biaxial stresses have strong influence on the fracture properties of glass. Thus, the fracture criterion by the stress intensity factor was questioned for the biaxial plane stress issues. It is confirmed that the tensile stress parallel to the crack plane is an important factor affecting crack arrest, while the compressive stress parallel to the crack plane contributes to crack opening.

Author
W Li Et Al
Origin
Dalian University, China
Journal Title
Key Eng Mat 297-300 2005 1617-1622
Sector
Special Glass
Class
S 3100

Request article (free for British Glass members)

Numerical Approach To Fracture Of Glass Under Biaxial Stress
Key Eng Mat 297-300 2005 1617-1622
S 3100
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.