Numerical And Experimental Study Of Blow And Blow For Perfume Bottles To Predict Glass Thickness And Blank Mold Influence

Glass forming to produce perfume bottles with specific thickness distribution profiles is based on trial and error and requires several tests in production line. The use of a numerical model aims to reduce the number of prototypes by performing virtual tests of the mould equipment and the process conditions. This article presents results of numerical simulations of the blow-and-blow forming process to predict glass thickness distribution. Correlation of the simulation results of the glass temperature with experimental infrared measurements on the glass skin and experimental validation of glass forming simulations and influence of the blank mould cavity in the thickness distributions of perfume bottles are provided. Finally, validation of the results of axisymmetrical and three-dimensional models for axisymmetric bottles defining a useful technique to use the right blank mould for desired thickness distribution while reducing the trial and error testing.

Author
A Biosca Et Al
Origin
El Masnou, Spain
Journal Title
Appl Glass Sci 10 October 2019 569-583
Sector
Container glass
Class
C 6200

Request article (free for British Glass members)

Numerical And Experimental Study Of Blow And Blow For Perfume Bottles To Predict Glass Thickness And Blank Mold Influence
Appl Glass Sci 10 October 2019 569-583
C 6200
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.