Numerical Analysis And Measurement Of Glass Flow In A Small Melting Furnace

Control of glass flow in a glass tank is a key technology in the melting process. The flow and temperature distributions of the glass melt greatly affect the quality of glass products. However, these phenomena have not been well understood due to the difficulty involved in the measurement as a result of the high temperature of the melt. A small melting furnace was developed that was heated by electrodes. The glass flow was measured and analysed by 3 D computer simulation. The numerical results show good agreement with the experimentally measured values. It is shown that it is possible to control the glass convection using a variety of the electric boosting conditions, the heat loss through walls and the charged glass batch. The quality of glass melt was evaluated by analysing the temperature histories of virtual particles the furnace was charged with.

Author
T Hiejima Et Al
Origin
Osaka Prefecture University, Japan
Journal Title
Glass Sci Technol 76 4 2003 155-165
Sector
General
Class
G 2717

Request article (free for British Glass members)

Numerical Analysis And Measurement Of Glass Flow In A Small Melting Furnace
Glass Sci Technol 76 4 2003 155-165
G 2717
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.