Nucleation And Crystallisation Behaviour Of Transparent, Erbium Iii Doped, Oxyfluoride Glass Ceramics For Active Photonic Devices

A new Er3+ doped oxyfluoride glass ceramic composition is reported based on published compositions but with improved glass stability on reheating. A series of heat treatments up to 168h at 394 deg C, close to Tg (glass transformation temperature), has been carried out and yielded visually transparent materials. X-ray diffractometry has shown that a fluorite structured phase with lattice parameter 0.574nm has crystallised after the heat treatment.

Author
L L Kukkonen Et Al
Origin
University Of Sheffield, Uk
Journal Title
Phys Chem Glasses 42 3 2001 265-273
Sector
Glass Ceramics
Class
GC 440

Request article (free for British Glass members)

Nucleation And Crystallisation Behaviour Of Transparent, Erbium Iii Doped, Oxyfluoride Glass Ceramics For Active Photonic Devices
Phys Chem Glasses 42 3 2001 265-273
GC 440
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.