Nucleation And Crystallisation Of An As2Se3 Undercooled Melt

The isothermal nucleation of an As2Se3 undercooled melt followed by crystallization and consequent melting was followed by DSC using a constant heading rate. The melting enthalpy was used to quantify the degree of conversion, α. Nonlinear regression analysis of the dependence of conversion on isothermal nucleation temperature and time was performed on the basis of classical nucleation theory assuming normal 3D growth. The parameters for the temperature dependence of nuclear rate and growth rate were determined by a three step process. First the simple parabolic model was used to estimate the maximum and the width of rate-temperature curve. Then, the obtained parabolic curves were fitted by theoretical ones. In the third step, the parameters obtained in the previous steps were used for nonlinear regression analysis of the experimental data. The kinetic barrier of crystal growth was found to be in agreement with the activation energy for viscous flow.

Author
M Liska Et Al
Origin
Joint Glass Centre Of Iic Sas, Slovakia
Journal Title
Phys Chem Glasses 53 6 Dec/2012 289-293
Sector
Special Glass
Class
S 3965

Request article (free for British Glass members)

Nucleation And Crystallisation Of An As2Se3 Undercooled Melt
Phys Chem Glasses 53 6 Dec/2012 289-293
S 3965
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.