Nuclear Microprobe And Optical Investigation Of Sparkling Wine Bottles

Glass bottles, used for sparkling wine, are treated with freon during manufacturing to harden the inside surface. Although this type of treatment normally improves the properties of the glass, in this case the occurrence of "egg" formations (egg-shaped rough areas) on distinct areas of bottles, as well as yeast sticking to the insides of bottles at specific areas, pointed to the possibility of different areas showing different properties in the same bottle. The question was whether the correct gas was used for the treatment, and secondly, whether the process was controlled well enough to obtain the correct properties for the inside of the glass. This paper presents results of an optical microscopy and nuclear microprobe (NMP) investigation.

Author
J Padayachee Et Al
Origin
Van De Graaff Group, South Africa
Journal Title
Science Direct Online: www.Sciencedirect.com/
Sector
Container glass
Class
C 2360

Request article (free for British Glass members)

Nuclear Microprobe And Optical Investigation Of Sparkling Wine Bottles
Science Direct Online: www.Sciencedirect.com/
C 2360
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 19 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.