Nox Reduction By Primary Measures: A Challenge For The European Glass Industry

This paper gives an overview of the present situation of NOx emission control in the glass industry. In particular, the different available techniques for NOx emission control are described as they are presently under discussion in the EU, at National and Community level, within the scope of the IPPC Directive 96/61.