Novel Visible Emission And Emchanism Investigation From Pbs Nanoclusters-Doped Borosilicate Glasses

Borosilicate glasses doped with PbO, ZnS, or PbS were fabricated to investigate the visible emissions observed in the PbO and ZnS co-doped glass. Several series of glassy systems were designed to investigate the mechanism of above visible emissions. The absorption, photoluminescence, photoluminescence excitation spectra, and lifetime measurements were used to characterise all the emissions.

Author
S Fan Et Al
Origin
S China University Technology, Guangzhou
Journal Title
Jacs 97 1 2014 173-178
Sector
Special Glass
Class
S 4149

Request article (free for British Glass members)

Novel Visible Emission And Emchanism Investigation From Pbs Nanoclusters-Doped Borosilicate Glasses
Jacs 97 1 2014 173-178
S 4149
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.