Novel Structural Behaviour Of Iron In Alkali-Alkaline-Earth-Silica Glasses

The combined effect of alkali and alkaline-earth ions on the redox, distribution, coordination and environment of Fe ions in alkali-alkaline-earth-silica glass has been studied using a multi-technique approach. Wet chemical analysis and Mossbauer, electron spin resonance (ESR), optical absorption and photoluminescence spectroscopies were utilised. Behaviour generally falls into two categories, which have been termed collective and selective.

Author
P Bingham Et Al
Origin
University Sheffield, Uk
Journal Title
Cr Acad Sci Chimie F-5 November 2002 787-796
Sector
Special Glass
Class
S 2839

Request article (free for British Glass members)

Novel Structural Behaviour Of Iron In Alkali-Alkaline-Earth-Silica Glasses
Cr Acad Sci Chimie F-5 November 2002 787-796
S 2839
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.