Novel Methods Of Mould Cooling

Emhart glass has developed a verti-flow mould cooling system that meets all the criteria for today's high-volume glassworks. With this system there is minimal noise and pollution and, as well as being economically advantageous for manufacturers, it is also safe and flexible for operators.