A Novel Glass Furnace Combining The Best Of Oxy-Fuel And Air-Fuel Melting

A novel furnace concept has been developed that combines oxy-fuel combustion over the unmelted batch and air-fuel combustion downstream. This hybrid furnace offers a number of advantages over both air-fuel and oxy-fuel furnaces. As compared to air-fuel, the hybrid furnace technology provides increased production, improved glass quality, fuel savings, better furnace temperature control, and a more stable batch pattern. As compared to 100% oxy-fuel, the hybrid furnace delivers similar production levels, improved glass quality, reduced levels of foam on the glass surface, and lower overall oxygen costs. The end result is that the hybrid furnace provides the means to achieve the lowest overall glass melting cost.

Author
M D'Agostini Et Al
Origin
Air Products & Chemicals Inc, Usa
Journal Title
Cesp 64 Conf Glass Problems 25 1 2004 153-166
Sector
General
Class
G 2821

Request article (free for British Glass members)

A Novel Glass Furnace Combining The Best Of Oxy-Fuel And Air-Fuel Melting
Cesp 64 Conf Glass Problems 25 1 2004 153-166
G 2821