Novel Bioactive Materials Derived By Bioglass: Glass-Ceramic A-W And Surface-Modified Ti Metal

It is shown in this study how bioactive glass-ceramic A-W with a high mechanical strength and bioactive surface-modified Ti metal with a high fracture toughness was derived from Bioglass®. Glass-ceramic A-W precipitating apatite and wollastonite was obtained by crystallization of a glass of a modified composition of Bioglass®. The resultant product showed a higher mechanical strength than human cortical bone, as well as bone-bonding ability. It was clinically used for various kinds of bone substitute such as artificial vertebrae and iliac crest. However, its fracture toughness is not so high as that of human cortical bone. By examining bone-bonding mechanism of Bioglass® and glass-ceramic A-W, it was found that a material capable of forming bonelike apatite on its surface in the living body bonds to living bone through the apatite layer. The apatite formation on a material in the living body can be evaluated even in a simulated body fluid in-vitro. On the basis of these findings, a Ti metal with high fracture toughness was conferred bone-bonding ability by surface modification with simple chemical and heat treatments. The resultant products are in clinical use for an artificial hip joint and spinal fusion devices.

Author
T Kokubo & S Yamaguchi
Origin
Chubu University, Japan
Journal Title
Int J Appl Glass Sci 7 2 2016 173-182
Sector
Special Glass
Class
S 4250

Request article (free for British Glass members)

Novel Bioactive Materials Derived By Bioglass: Glass-Ceramic A-W And Surface-Modified Ti Metal
Int J Appl Glass Sci 7 2 2016 173-182
S 4250
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.