Novel 3D Composites With Highly Flexible Behaviour Based On Chitosan And Bioactive Glass For Biomedical Applications

Scaffolds with a 3D cellular solid structure have been studied intensively for tissue engineering. These materials should have adequate porosity, appropriate pore size, interconnectivity, and mechanical behaviour compatible with the features of native tissue, allowing cell activities. In this work, novel flexible 3D composite foams of chitosan (CH) combined with bioactive glass (BG) in 1:0 and 1:1 ratios by a foaming method were developed.

Author
T Martins Et Al
Origin
Federal University Minas Gerais, Brazil
Journal Title
Materials Chemistry & Physics 189 2017 1-11
Sector
News Items
Class
N 3751

Request article (free for British Glass members)

Novel 3D Composites With Highly Flexible Behaviour Based On Chitosan And Bioactive Glass For Biomedical Applications
Materials Chemistry & Physics 189 2017 1-11
N 3751
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.