Novaxion'S Latest Swabbing Tobot Is Integrated Onto Emhart Machine

This article discusses how the latest version of a swabbing robot has been installed on an Emhart AIS machine and explains the benefits it brings to product quality, profitability and operator well-being.

Author
C Duplan
Origin
Novaxion, France
Journal Title
Glass International February 2018 55, 57
Sector
Container glass
Class
C 5970