Nonlinear Optical Susceptibilities Of High-Index Glasses

Results of degenerate four-wave mixing measurements of nonresonant nonlinearities in a variety of high-index lead and bismuth containing oxide glasses and the chalcogenide arsenic sulphide are reported.

Author
D W Hall Et Al
Origin
Corning Glass Works
Journal Title
Appl Phys Lett 1989 54 14 1293-1295